Tabulky Am/V

Publikováno dne 30. 3. 2010

Válcované profily I

Profil  č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
803464020,30442
1003023490,37050
1202683090,43958
1402402760,50266
1602202520,57574
1802002290,64082
2001852120,70990
2201711960,77598
2401601830,844106
2601491690,906113
2801391580,966119
3001311491,030125
3201231401,090131
3401171331,150137
3601101251,210143
3801051191,270149
4001001131,330155
425941071,410
450891011,480170
47584951,550
50081911,630185
55075851,800
60067761,92

Válcované profily IPE

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
803724290,32846
1003343880,40055
B03153600,47564
1402913360,55173
1602693100,62382
1802552920,69891
2002342690,768100
2202212540,848110
2402052360,922120
2701972271,040135
3001882151,160150
3301752001,250160
3601631861,350170
4001521731,470180
4501431621,610190
5001331501,74200
5501241401,880210
6001151292,001220

Válcované profily IE

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
804335090,264
1002793250,33555
1202693130,39664
1402633050,45773
1602572980,51981
1802482870,58090
2002432800,650100
2202352720,720110
2402202530,765115
2702132440,855125
3002012310,935135
3301882141,010140
3601751991,085145
4001671901,195
4501601801,330
5001491671,46

Válcované profily IPB (HE-B)

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
1002002180,567100
1201822020,686120
1401671870,805140
1601541690,918160
1801431591,040180
2001331471,150200
2201251401,270220
2401181301,380240
2601141271,500260
2801111241,620280
3001051161,730300
320981101,770300
340931061,810300
360891021,850300
40083971,930300
45079932,030300
50076892,120300
55076872,220300
60075862,320300
65074852,420300
70073822,52300
80072812,71300
90070782,91300
100070783,11300

Válcované profily IPBI (HE-A)

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
1002502650,561100
1202502640,677120
1402352530,794140
1602222340,906160
1802112251,020180
2002002121,140200
2201821961,260220
2401671781,370240
2601601711,480260
2801541641,600280
3001431521,720300
3201291421,760300
3401211351,790300
3601141281,830300
4001051202,110300
450961132,210300
500911071,910300
550901042,010300
600891022,310300
650871002,410300
70085962,5300
80084942,7300
90081902,9300
100081893,1300

Válcované profily IPBv (HE-M)

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
1001001160,619
120951110,738
140911060,857
160871000,970
18083961,090
20080921,20
22077891,32
24063731,46
26062711,57
28061701,69
30051601,83
320/30569791,78
32050601,87
34050601,90
36051611,93
40052612,00
45054632,10
50054632,18
55056642,28
60057652,37
65058662,47
70059672,56
80061682,75
90062692,93
100064703,13

Válcované profily U

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
802412840,31245
1002372760,37250
1202212550,43455
1402102400,48960
1601982280,54665
1801892180,61170
2001822050,66175
2201711920,71880
2401641830,77585
2601531730,83490
2801491670,89095
3001451620,950100
3201171300,982
3501211351,047
3801241381,110
4001161291,182

Válcované profily UE

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
502893410,17832
652853330,21436
802893340,26040
1002883300,31446
1202773160,36852
1402713080,42258
1602693040,48664
1802612950,54070
2002542860,59476
2202432730,64882
2402322610,71090
2702232500,78595
3002122380,805100

Válcované profily UPE

Profil č.Am/V (m-1)Obvod
(m2/bm)
Šířka pásnice
(mm)
ze 3 stranze 4 stran
502863380,22032
6529634436
802993430,34240
1002953360,40146
1202823210,46052
1402823180,51958
1602733080,55764
1802642980,63670
2002612940,69576
2202482790,75482
2402372660,81090
2702272540,88995
3002162410,968100

Válcované profily L

Profil č.Am/V
(m-1)
Obvod
(m2/bm)
30x30x 36900,12
30x30x 45290,12
35x35x 36860,14
35x35x 45240,14
40x40x 36380,15
40x40x 44870,15
40x40x 53960,15
45x45x 36390,17
45x45x 44870,17
45x45x 53930,17
50x50x 44880,19
50x50x 54210,19
50x50x 63340,19
55x55x 53950,21
55x55x 63430,21
60x60x 63330,23
60x60x 82550,23
65x65x 63320,25
65x65x 82540,25
70x70x 63310,27
70x70x 72870,27
70x70x 82520,27
80x80x 63320,31
80x80x 82520,31
80x80x 102050,31
90x90x 63330,35
90x90x 82520,35
90x 90x 102050,35
100x100x 63300,39
100x100x 82520,39
100x100x 102030,39
100x100x 121720,39
110x110x 82510,43
110x110x 102020,43
120x120x 82510,47
120x120x 102030,47
120x 120x 121710,47
125x125x 82490,49
125x125x 102020,49
125x125x 121700,49
125x125x 141470,49
130x130x 121700,51
130x130x 141470,51
140x140x 102020,55
140x140x 121700,55
140x140x 141470,55
160x160x 102010,63
160x160x 121690,63
160x160x 141460,63
160x160x 161290,63
180x180x 121660,70
180x180x 141430,70
200x200x 161260,78
200x200x 201020,78

Trubky (sloupy)

Průměr
(mm)
Tl. stěny
(mm)
Am/V
(m-1)
Obvod
(m2/bm)
222,54530,069
2233870,069
223,53410,069
2243070,069
252,54450,079
2533800,079
253,53340,079
2542980,079
254,52720,079
2582510,079
282,54410,088
2833740,088
283,53280,088
2842920,088
284,52660,088
2852450,088
322,54340,101
3233690,101
323,53220,101
3242860,101
324,52590,101
3252380,101
325,52200,101
3262060,101
352,54320,110
3533650,110
353,53190,110
3542830,110
354,52560,110
3552340,110
355,52160,110
3562020,110
3571790,110
35101410,110
382,54290,119
3833630,119
383,53160,119
3842800,119
384,52530,119
3852310,119
385,52130,119
3861990,119
3871700,119
3881590,119
442,54240,140
4433580,140
443,53110,140
4442760,140
444,52480,140
4452260,140
445,52080,140
4461930,140
4471700,140
4481530,140
4491410,140
44101300,140
44121150,140
512,54210,160
5133550,160
513,53080,160
5142720,160
514,52450,160
5152220,160
515,52050,160
5161900,160
516,51770,160
5171660,160
5181490,160
5191360,160
51101250,160
51121100,160
542,54210,170
5433540,170
543,53070,170
5442710,170
544,52430,170
5452210,170
545,52030,170
5461880,170
546,51760,170
5471660,170
5481470,170
5491350,170
5733530,179
573,53050,179
5742700,179
574,52420,179
5752200,179
575,52020,179
5761870,179
576,51750,179
5771640,179
5781470,179
5791330,179
57101220,179
6033520,188
603,53040,188
6042690,188
604,52410,188
6052190,188
605,52010,188
6061860,188
606,51740,188
6071620,188
6081450,188
6091320,188
60101210,188
60121050,188
7033490,220
703,53020,220
7042660,220
704,52380,220
7052160,220
705,51990,220
7061830,220
706,51700,220
7071590,220
7081420,220
7091280,220
70101170,220
70121010,220
7633480,239
763,53000,239
7642650,239
764,52370,239
7652140,239
765,51970,239
7661820,239
766,51690,239
7671580,239
7681410,239
7691270,239
76101160,239
76121000,239
7614880,239
833,52990,261
8342630,261
834,52360,261
8352130,261
835,51950,261
8361810,261
8371680,261
8381570,261
8391390,261
83101150,261
8312980,261
8314870,261
893,52980,280
8942620,280
894,52340,280
8952130,280
895,51950,280
8961790,280
8971660,280
8981560,280
8991380,280
89101140,280
8912970,280
8916770,280
953,52960,298
9542630,298
954,52340,298
9552130,298
955,51930,298
9561790,298
9571550,298
9581370,298
9591240,298
95101120,298
9512960,298
9516760,298
1023,52980,320
10242610,320
1024,52330,320
10252120,320
1025,51930,320
10261780,320
10271540,320
10281370,320
10291230,320
102101120,320
10212950,320
10216750,320
10218680,320
10842600,339
1084,52330,339
10852100,339
1085,51930,339
10861780,339
10871540,339
10881360,339
10891220,339
108101110,339
10812950,339
10814830,339
10816740,339
10818680,339
10820620,339
11442600,358
1144,52320,358
11452100,358
1145,51910,358
11461760,358
11471520,358
11481360,358
11491220,358
114101100,358
11412940,358
11414820,358
11416740,358
11418670,358
11420620,358
12142590,380
1214,52310,380
12152100,380
1215,51910,380
12161760,380
12171520,380
12181350,380
12191210,380
121101100,380
12112930,380
12114820,380
12116730,380
12118660,380
12120610,380
12742580,399
1274,52320,399
12752090,399
1275,51910,399
12761760,399
12771520,399
12781340,399
12791200,399
127101090,399
12712930,399
12714810,399
12716720,399
12718660,399
12720600,399
12722560,399
13342590,418
1334,52300,418
13352090,418
1335,51910,418
13361760,418
13371520,418
13381340,418
13391200,418
133101090,418
13312930,418
13314810,418
13316720,418
13318650,418
13320600,418
13322550,418
13325500,418
1524,52290,477
15252080,477
1525,51900,477
15261750,477
15271510,477
15281330,477
15291190,477
152101080,477
15212910,477
15214800,477
15216710,477
15218640,477
15220590,477
15222540,477
15225490,477
1594,52300,499
15952070,499
1595,51890,499
15961740,499
15971500,499
15981320,499
15991190,499
159101080,499
15912910,499
15914790,499
15916700,499
15918640,499
15920580,499
15922540,499
15925490,499
15928440,499
1684,52290,528
16852070,528
1685,51890,528
16861740,528
16871500,528
16881320,528
16891180,528
168101070,528
16812910,528
16814790,528
16816700,528
16818630,528
16820580,528
16822530,528
16825480,528
16828440,528
1945,51880,609
19461730,609
19471490,609
19481310,609
19491170,609
194101060,609
19412900,609
19414780,609
19416690,609
19418620,609
19420570,609
19422520,609
19425470,609
19428430,609
19432380,609
21961720,688
21971490,688
21981310,688
21991170,688
219101060,688
21912890,688
21914770,688
21916680,688
21918610,688
21920560,688
21922520,688
21925460,688
21928420,688
21932380,688
2456,51590,769
24571480,769
24581300,769
24591160,769
245101050,769
24512890,769
24514760,769
24516680,769
24518610,769
24520560,769
24522510,769
24525450,769
24528410,769
24532370,769
24536340,769
27371480,857
27381300,857
27391160,857
273101050,857
27312880,857
27314760,857
27316670,857
27318610,857
27320550,857
27322510,857
27325450,857
27328410,857
27332360,857
27336330,857
3246,51581,017
3247,51371,017
32491151,017
324101041,017
32412871,017
32414761,017
32416671,017
32418601,017
32420541,017
32422501,017
32425441,017
32428401,017
32432361,017
32436321,017
37791151,184
377101041,184
37712871,184
37714751,184
37716661,184
37718591,184
37720541,184
37722491,184
37725441,184
37728401,184
37732351,184
37736321,184

Válcované profily U svařené proti sobě

2 x U profil č.Am/V (m-1)Obvod
(m2/bm)
ze 3 stranze 4 stran
501251780,252
651191660,298
801151560,34
1001121490,4
1201041360,46
140991280,52
160951220,58
180911150,64
200871100,70
220821030,76
24078980,82
26074930,88
28072890,94
30069861,00